SAMARTH ENTERPRISES
Premium Ferro Molybdenum (FeMo 60-70%) – High Molybdenum 65-75%, Low Impurities Alloying Additive for High-Strength Low-Alloy Steel, Stainless Steel, Tool Steel & Superalloys | Improves Corrosion Resistance, Weldability, High-Temp Strength & Hardenability
AED 81,000.00 - 90,000.00
/Ton
MOQ: 22 Tons
Lead Time
Quantity (Pieces)
22 - 100
101 - 500
>500
Lead Time (Days)
18
33
Negotiated
Get the latest update on price, transportation and customization.
AED 90,000.00
SKU
SAMARTH0009
Basic Info
| Product Type | Ferro Molybdenum |
| HSN | 72027000 |
| Chemical Composition | Fe-Mo (60-75% Mo) |
| Impurity Levels (P+S) | S<0.05%, P<0.01% |
| Density (g/cm³) | 9.0-10.0 |
| Melting Point (°C) | 1500-1700°C |
| Particle Size | 10-100mm |
| Deoxidizing Power | Moderate |
| Desulfurizing Ability | Low |
| Alloying Element Role | Hardenability |
| Edges | Lumpy |
| HS Code | 7202.7 |
| Moisture Content | <0.04% |
| Applications | Tool steels |
| Country of Manufacture | India |
Packaging & Delivery
| Product Weight | 10.00 Kg |
| Shipping Port | Mormugao Port |
About Us



Mission & Vision


Our Products


Core Values

Why Choose Us

Description
{{block class="Magento\Framework\View\Element\Template" image="" text=" About Us" template="MGS_Fbuilder::widget/imagetext/imagetext.phtml"}}{{block class="Magento\Framework\View\Element\Template" type="single" image="/2/_/2_50.jpg" alt="" alt_after="" template="MGS_Fbuilder::widget/image/single.phtml"}} {{block class="Magento\Framework\View\Element\Template" type="single" image="/8/_/8_57.jpg" alt="" alt_after="" template="MGS_Fbuilder::widget/image/single.phtml"}} {{block class="Magento\Framework\View\Element\Template" type="single" image="/3/_/3_66.jpg" alt="" alt_after="" template="MGS_Fbuilder::widget/image/single.phtml"}} {{block class="Magento\Framework\View\Element\Template" image=" " text=" Mission & Vision" template="MGS_Fbuilder::widget/imagetext/imagetext.phtml"}}{{block class="Magento\Framework\View\Element\Template" type="single" image="/4/_/4_74.jpg" alt="" alt_after="" template="MGS_Fbuilder::widget/image/single.phtml"}} {{block class="Magento\Framework\View\Element\Template" type="single" image="/5/_/5_68.jpg" alt="" alt_after="" template="MGS_Fbuilder::widget/image/single.phtml"}} {{block class="Magento\Framework\View\Element\Template" image="" text=" Our Products" template="MGS_Fbuilder::widget/imagetext/imagetext.phtml"}}{{block class="Magento\Framework\View\Element\Template" type="single" image="/6/_/6_63.jpg" alt="" alt_after="" template="MGS_Fbuilder::widget/image/single.phtml"}} {{block class="Magento\Framework\View\Element\Template" type="single" image="/7/_/7_57.jpg" alt="" alt_after="" template="MGS_Fbuilder::widget/image/single.phtml"}} {{block class="Magento\Framework\View\Element\Template" image=" " text=" Core Values" template="MGS_Fbuilder::widget/imagetext/imagetext.phtml"}}{{block class="Magento\Framework\View\Element\Template" type="single" image="/1/0/10_42.jpg" alt="" alt_after="" template="MGS_Fbuilder::widget/image/single.phtml"}} {{block class="Magento\Framework\View\Element\Template" image="" text=" Why Choose Us" template="MGS_Fbuilder::widget/imagetext/imagetext.phtml"}}{{block class="Magento\Framework\View\Element\Template" type="single" image="/1/1/11_40.jpg" alt="" alt_after="" template="MGS_Fbuilder::widget/image/single.phtml"}} |
| Profie Name | Siddhesh Katkar |
| Company Name | |
| Shop URL | https://www.kobray.com/marketplace/seller/profile/shop/Samarth |
| Shop Title | |
| Company Locality | |
| Company Description | |
| Shipping Policy | |
| Return Policy | |
| Contact Number |
Sales Service
|
|
(872.93 kB) | Download |
Write Your Own Review